Titanium alloy powder can absorb oxygen during handling, storage, and additive manufacturing, degrading the mechanical properties of printed parts and limiting reuse. Researchers treated oxidized spherical Ti-6Al-4V powder with calcium, followed by acid pickling and drying, then examined individual particles across multiple length scales.
Atom-probe measurements found that the oxidized powder’s roughly 10-nanometer oxide region fell below 5 nanometers after treatment. Oxygen in the underlying alloy matrix decreased from about 3.2 to 0.5 atomic percent. A calcium–oxygen reaction layer and a narrow calcium–titanium–oxygen interface directly supported a surface-mediated oxygen-transfer mechanism.
The work supplies mechanistic evidence for rejuvenating high-oxygen titanium feedstock rather than discarding it. The paper does not establish economics, repeated recycle loops, powder-flow behavior, or the mechanical performance of parts printed from the treated material. Several authors also disclosed a related Singapore patent application.
Source record: Brightwire summarized and evaluated this development from the linked primary material. Read the original for complete context.
Read at npj Materials Degradation