Researchers designed ten alkali-activated concrete mixtures that cut ground-granulated blast-furnace slag to 20% and substituted waste charcoal ash, ceramic powder, basalt powder and other mineral residues. They compared water, heat and steam-water curing and measured workability, mechanical strength, sulfate resistance and environmental performance.

After 28 days, the control, metakaolin and waste-ceramic mixtures reached compressive strengths of 87, 75 and 70 megapascals. Quartz-powder and waste-basalt blends increased flexural strength by as much as 44% and 25%, while selected metakaolin and quartz mixtures also showed stronger resistance to sodium and magnesium sulfate attack.

These are controlled laboratory mixtures rather than field structures, and the best-performing formulations did not lead every measure. Local waste chemistry, alkaline activators, curing energy and full life-cycle accounting will determine whether the reported performance and sustainability gains survive commercial scaling.

Source record: Brightwire summarized and evaluated this development from the linked primary material. Read the original for complete context.

Read at Scientific Reports